Additions of 0.2–0.6 wt% Y2O3 can improve oxidation resistance of alloys.

Additions of 0.2–0.6 wt% Y2O3 can improve adhesion of oxide scale.

Additions of 0.2–0.6 wt% Y2O3 can improve relative density of alloys.

Addition of Y2O3 can decrease hardness and bending strength of alloys.