Hydrothermal recovery of asphalt from asphalt concrete was investigated.
Refraining from stirring during treatment and a continuous stirring during cooling were the optimum stirring conditions.
The other optimum conditions were 300 °C, 2 mL/g, 450 rpm, and 3 h.
Recycled aggregate of asphalt content smaller than 0.5% could be produced.