Bi2WO6 was improved to possess ultra-high Curie temperature by experiment.
The highest depolarization temperature is around 940 °C.
The symmetry group of ultra-high Curie temperature Bi2WO6 is Aba2 (41).
The structure change with Mn doping was studied by ab initio and refinement calculations.