LiMn0.85Fe0.15PO4/C microspheres are prepared by a wet-milling-spray drying method. LiMn0.85Fe0.15PO4/C particles are in porous-hollow form coated with a carbon layer. Porous-hollow LiMn0.85Fe0.15PO4/C microspheres give good electrochemical performance.