The submicron-sized WC particles are bound with WC-Co powders by ball mill method.
The even distribution of WC particles at the interfaces of WC-Co splats is achieved.
The presence of WC particles changes the stress state at the splats' interfaces.
The WC particles at the splats' interface inhibit the propagation of microcracks.
The addition of WC particles enhances the microhardness and sliding wear resistance.