Effects of Pt Particle Size on Hydrogen Storage on Pt-Doped Metal鈭扥rganic Framework IRMOF-8
详细信息    查看全文
  • 作者:Lifeng Wang ; Nicholas R. Stuckert ; Hao Chen ; Ralph T. Yang
  • 刊名:Journal of Physical Chemistry C
  • 出版年:2011
  • 出版时间:March 24, 2011
  • 年:2011
  • 卷:115
  • 期:11
  • 页码:4793-4799
  • 全文大小:915K
  • 年卷期:v.115,no.11(March 24, 2011)
  • ISSN:1932-7455
文摘
A series of Pt-doped IRMOF-8 samples with different Pt catalyst sizes have been prepared via organometallic chemical-vapor deposition (CVD). The Pt catalyst size effects on the spillover storage on IRMOF-8 (or any MOF) were studied for the first time. Our studies showed that the Pt catalyst size is a crucial factor determining whether a significant enhancement in storage can be achieved in the hydrogen spillover system at ambient temperature. Compared to undoped IRMOF-8, the spillover storage capacities on Pt-doped IRMOF-8 samples were enhanced by factors ranging from 1.1 to 1.9 because of different Pt catalyst sizes. The doped Pt size was controlled by varying the CVD conditions to yield mean sizes of 2.2, 3.9, and 9.1 nm, and the results showed that smaller sizes were needed for spillover. Temperature-programmed desorption of dosed H2/D2 further shed light on the mechanism of spillover and reverse spillover, confirming undercoordinated sites on the particle-enhanced spillover.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700