摘要
Wastes generated from the Bayer’s process serve as valuable resources for aluminum, vanadium, gallium, etc. This work aims to develop a environmentally acceptable and low-cost chemical leaching-cumpurification method for the recovery of vanadium sludge of Indian alumina plant (10–12% V2O5) and synthesize vanadium pentaoxide. The efficiency of leaching was evaluated by various lixiviants like acidified water, H2SO4, soda and NaOH against variation in pulp density and temperature. Maximum extraction (96%) vanadium was achieved using acidified water leaching at above ambient temperature in 1 h with 200 g/L pulp density following diffusion control model. Finally, the vanadium rich leach liquor was purified by steps of adsorption/precipitation etc., to remove with iron and silica to get vanadium pentaoxide. A high purity product of 99% V2O5 was obtained by allowing the adsorption at acidic pH followed by desorption and precipitation at 90°C.