At 75 °C, the early-term strength of cement decreased with the increasing MK content.
At 75 °C, the set cement with more MK showed higher long-term strength.
Beyond 150 °C, samples M40 to M60 presented good strength in all test ages.
Hydration products and structure would influence strength and porosity of cement.
High dosage of MK cement is suitable for corrosion and high temperature conditions.