Zr was employed as an impurity getter in MG-Si.
Presence of Zr in MG-Si contributes to efficient removal of most impurities.
99.9% of the added Zr could be removed after HCl + HF or HF leaching.
HCl + HF is the optimal lixiviant for purification of MG-Si with Zr addition.