The B50 of NOG steels was evaluated via texture for different rolling processes.
On comparison to all processes used, the cross-rolling led to highest average B50.
Cross-rolling enhances Goss and γ-fiber after annealing.
The better B50 values were obtained for symmetrical and cross-rolling processes.
For asymmetric rolling process, cylinder diameter ratio changed slightly the texture.