Electrocrystallization of CaP electrodeposition on CP-Ti and SLM-Ti. Both samples exhibit diffusion controlled 3D instantaneous nucleation mechanism. Lower overpotential was obtained on SLM-Ti in initial electrodeposition stage. Lower overpotential on SLM-Ti is attributed to more surface defects.