Preparation, microstructure and electrical properties of Li1.4Al0.4Ti1.6(PO4)3 nanoceramics
详细信息    查看全文
文摘
NASICON-type Li1.4Al0.4Ti1.6(PO4)3 solid electrolytes were prepared by various processes, such as crystallization of glasses, spark plasma sintering (SPS) and conventional sintering process from nanosized precursor powders synthesized by a sol–gel route. The experimental results showed that grain size and relative density were the main factors determining the ionic conductivity of the bulk materials. The SPS technique produced ceramics with nearly 100 % of the theoretical density. Maximum room temperature conductivities, 1.39 ¡Á 10−3 S cm−1 and 1.12 ¡Á 10−3 S cm−1 of grain boundary conductivity and total conductivity, respectively were obtained which were the highest values for Li+ inorganic oxide conductors as reported. Crystallization of ceramics from a glass was also certified as a favorable route to fabricate a bulk material with high conductivity.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700