摘要
针对福建某低品位铜矿石,通过对矿物性质及原工艺流程的诊断分析,采用"粗磨—快速浮选—快浮尾矿异步浮选—粗精矿再磨再选"的联合工艺,能有效保证了已解离的目的矿物优先回收,同时还使得难选铜矿物及含铜连生体矿物得到充分回收。新工艺流程获得了含铜24.09%、含金6.48 g/t、铜回收率为92.69%、金回收率为60.54%的铜精矿,铜回收率提高了3.87个百分点,金回收率提高了13.61个百分点。
After the diagnosis and analysis on mineral properties and original process flow of a low-grade copper ore from Fujian, the process flow involving rough grinding, rapid flotation, asynchronous flotation of tailings of rapid flotation, re-grinding and re-separation of rough concentrate in sequence was applied to effectively ensure the preferential recovery of dissociated target minerals as well as ample recovery of refractory copper minerals and copper-bearing coenobium minerals. After application of the new process flow, the copper concentrate with copper content of 24.09%, gold content of 6.48 g/t, copper recovery ratio of 92.69% and gold recovery ratio of 60.54% was obtained. Thus the copper recovery ratio increased by 3.87 percentage points, and the gold recovery ratio increased by 13.61 percentage points.
引文
[1]印万忠,李强.国内外金属矿山难选矿选冶新技术进展[C]//2008年全国金属矿山难选矿及低品位矿选矿新技术学术研讨与技术成果交流暨设备展示会论文集,深圳,2008:33-70.
[2]李广.提高某选厂铜回收率的新工艺研究[D].武汉理工大学,2009:12.
[3]胡海祥,李广,李骥.提高某铜选厂一段选铜回收率的新工艺试验研究[J].矿业研究与开发,2010,30(4):22-25.
[4]朱建光.浮选药剂[M].北京:冶金工业出版社,1993:4.
[5]纪翠翠.高碱性氧化铜矿石的氨浸—萃取试验研究[D].昆明:昆明理工大学,2009:10.
[6]王政德.提高某铜矿中银回收率的试验研究[J].矿产保护与利用,1996,16(2):43-45.
[7]紫金矿业集团股份有限公司.低品位硫化铜矿的选矿方法:201510789291.1[P].2016-01-27.